A 20 W fibre laser focused to a 46 µm spot puts about 1.2 MW/cm² on the workpiece on average, and roughly 3.9 × 10⁸ W/cm² in each 100 ns pulse. Nothing else in a job shop concentrates energy like that. The same beam, with the same optics, can grow a 100 nm oxide film that turns stainless steel gold, melt a shallow pool that resolidifies black, or excavate 20 µm of material per pass — and the difference between those three outcomes is a handful of settings that most operators inherit as a recipe from the last person at the machine.
That is the problem with laser marking as an engineering discipline: it is usually taught as a settings list. But a settings list does not transfer between a 20 W Q-switched source and a 30 W MOPA, between a 110 mm and a 254 mm lens, between 304 and 430 stainless, or between one lot of black polycarbonate and the next. What transfers is the arithmetic behind the mark: how the spot is formed, how much energy each pulse carries, how much of it the material absorbs, and what the absorbed energy does.
This guide works through that chain, then follows it into the parts of marking that actually decide whether a job ships — colour repeatability, anodised aluminium, polymer additives, direct-part-mark grading, fatigue, fume and cost. The focus is the marking most shops actually do: serial numbers, logos, UDI codes, tool tags, nameplates and the occasional decorative colour mark.
What the beam actually does
Laser marking is not one process. It is at least four, distinguished by peak intensity and interaction time.
Annealing keeps the surface below melting. The pulse train heats a thin surface layer in air; oxygen diffuses in and grows an oxide film tens to hundreds of nanometres thick. The film interferes with reflected light and produces colour or a dark mark. No material is removed, so the surface stays flat and the mark cannot be felt. The trade calls this "annealing", and it is often described as carbon being drawn to the surface; on stainless steel the dominant mechanism is oxide growth, and the colour is thin-film interference, not carbon.
Melting raises the surface above the liquidus. The pool flows, oxidises and resolidifies with a different microstructure and roughness. A melt mark is usually dark grey to black, slightly raised or recessed depending on surface tension, and visible in raking light.
Ablation takes the surface above vaporisation. Material leaves as vapour, droplets and plasma; each pass removes a controlled depth. This is what most people mean by engraving: a tactile, recessed mark, typically 5–50 µm deep per pass on stainless, with a recast layer and a heat-affected zone at the walls.
Carbonisation and foaming are the polymer analogues. Aromatic polymers char to a dark mark; polyolefins and some filled grades foam into a light mark against a dark substrate. Neither is ablation in the metal sense — the chemistry is decomposition, and the fume is the process by-product that has to be extracted.
Which regime you get is set by intensity, not by the power dial alone. A 20 W beam spread over a 1 mm spot is a heater; the same 20 W in a 46 µm spot is a cutting tool.
The optics decide the mark before the settings do
A fibre marker is a galvanometer scanner plus an f-theta lens. The laser is collimated into the scanner, two mirrors steer the beam, and the f-theta lens focuses it onto a flat field. Three numbers follow from that geometry: spot size, depth of focus and field size.
For a collimated beam of diameter D focused by a lens of focal length f, the 1/e² spot diameter is
where \lambda is the wavelength and M^2 is the beam propagation ratio. The depth of focus for a permitted fractional growth \varepsilon in spot diameter is
At \varepsilon = 5\% this collapses to \mathrm{DOF} \approx 0.5\, d_0^2/(M^2\lambda).
Put numbers in. A typical 20 W marker has a 7 mm output beam and M^2 \approx 1.5 at 1064 nm:
f-theta lens · Spot diameter · DOF (±5% growth) · Field (approx.)
110 mm · 32 µm · ±0.16 mm · 70 × 70 mm
160 mm · 46 µm · ±0.34 mm · 110 × 110 mm
210 mm · 61 µm · ±0.58 mm · 140 × 140 mm
254 mm · 74 µm · ±0.85 mm · 175 × 175 mm
The field grows roughly in proportion to f, the spot grows with it, and the depth of focus grows with the square. That is the trade. A 110 mm lens gives fine detail and a third of a millimetre of focus latitude; a 254 mm lens covers a nameplate but puts a 74 µm spot on it, which is wider than the stroke of 6 pt text.
The same equation explains why 20 µm spots are expensive. To reach 20 µm at 160 mm with M^2 = 1.1 you need an 11.9 mm beam entering the lens; with M^2 = 1.5 you need 16.3 mm. Either way the beam expander, the scanner aperture and the lens all have to be bigger, and the depth of focus falls to ±86 µm at 5% growth. On a machined surface with 0.1 mm of flatness error, that budget is already gone. This is why fine marking on curved or unfinished parts needs either a longer lens with a bigger spot or a Z-map/autofocus.
Focus is the first variable, not the last. On a flat plate, a 0.3 mm focus error at a 46 µm spot is a visible change in line width and darkness. On a curved part, the mark changes across the field unless the surface is at constant height or the software compensates. Annealing is the exception: it is deliberately run defocused, typically 3–5 mm above the surface, to spread the heat and avoid vaporisation.
Pulse arithmetic: energy, fluence, intensity
Average power is the least useful number on the datasheet. What the material sees is pulse energy, peak power, fluence and intensity.
Take 20 W at 30 kHz, 100 ns, on a 46 µm spot (A = 1.7 \times 10^{-5} cm²):
- E_p = 20/30{,}000 = 0.67 mJ
- P_{peak} = 0.67\,\text{mJ}/100\,\text{ns} = 6.7 kW
- F = 0.67\,\text{mJ}/1.7\times10^{-5}\,\text{cm}^2 \approx 39 J/cm²
- I_{peak} \approx 3.9 \times 10^8 W/cm²
- I_{avg} = 20/1.7\times10^{-5} \approx 1.2 \times 10^6 W/cm²
Thirty-nine joules per square centimetre is far above the ablation threshold of stainless steel for nanosecond pulses, which is why a 20 W marker can engrave metal at all. It is also why the same laser can destroy a thin foil if the operator treats "20 W" as a gentle setting.
The speed limit nobody quotes
The scanner may be specified at 7,000 mm/s, but the beam cannot move faster than the pulse train can deposit a continuous line. Adjacent pulses land a distance
apart. For overlap, p < d_0, which gives a hard ceiling:
At 30 kHz and a 46 µm spot, v_{max} = 1.39 m/s. Above that the line becomes a row of dots: at 2 m/s the pitch is 67 µm against a 46 µm spot, a 44% gap, and the mark looks dashed under magnification even if it looks solid to the eye. A 100 kHz source with the same spot raises the ceiling to 4.6 m/s. This is the entire practical value of high repetition rate for marking: not "more power", but a faster continuous line.
Hatch, area rate and time
For a filled area, the hatch spacing h sets how much of the surface is covered. The area rate is
At 1 m/s with 0.02 mm hatch, that is 20 mm²/s: a 10 × 10 mm solid block takes 5 s of beam time, before scanner jumps and before the part is loaded. Tighten the hatch to 0.002 mm for colour work and the same block takes 50 s. Colour is expensive because it is a 100% coverage process at low speed.
Line energy and melt depth
Absorbed line energy is A \cdot P/v. At 1 m/s and 35% absorptance, a 20 W beam deposits 7 J/m. Melting stainless takes about
so 7 J/m can melt a cross-section of 9.3 \times 10^{-10} m². Spread across a 46 µm wide track, that is about 20 µm deep per pass. Conduction takes some of it, and the plasma takes more, so the real depth is lower — but the order of magnitude is right, and it explains why 20 W marks and engraves but does not cut 3 mm plate. For comparison, a MIG weld runs at 300–800 J/mm of line energy; marking runs at 0.02 J/mm, four orders of magnitude lower.
Absorptance: why stainless is easy and copper is not
At 1064 nm, the difference between a metal that marks beautifully and one that fights the beam is mostly absorptance.
Material · Absorptance at 1064 nm (clean, room temperature)
Stainless steel 304/316 · 0.30–0.45
Mild steel · 0.30–0.40
Titanium · 0.20–0.35
Brass · 0.10–0.20
Aluminium · 0.05–0.10
Copper · 0.02–0.08
The same metals at 10.6 µm — the CO₂ wavelength — sit near 0.02–0.10, which is why CO₂ lasers do not mark bare metal and why fibre lasers displaced them for metal work. Absorptance also rises with temperature and with surface roughness, and an oxide or oil film changes it again. Two batches of the same stainless can mark differently because one was passivated and the other was not.
The practical consequences are direct. Stainless steel at 35% coupling needs about 7 J/m absorbed to melt, and a 20 W source delivers that at 1 m/s. Copper at 5% needs seven times the energy for the same melt, and its high thermal conductivity pulls heat away from the spot, so a 20 W 1064 nm marker produces a weak, unstable mark. Green (532 nm) or blue (450 nm) sources couple 40–60% into copper and are the production answer; for thin plating and busbars, a high-peak-power MOPA at 1064 nm can also work, at the cost of a narrow window.
Stainless steel: three marks from one machine
Stainless is the reference material for fibre marking because the same 20 W source can produce all three mark types.
Annealing. Defocus 3–5 mm, run high frequency and relatively low peak power, and move slowly enough to heat without vaporising. The surface grows an oxide film; the mark is dark grey to black, flat to the touch and resistant to rubbing because it is part of the surface, not a coating. Typical starting point on 304 with a 20 W Q-switched source: 40–60% power, 15–250 mm/s, 20–50 kHz, 0.015–0.025 mm hatch, one or two passes, focus +3 to +5 mm.
Etching. Focus on the surface, moderate frequency, moderate speed. The surface melts and resolidifies; the mark is grey-white to dark, slightly tactile and 5–20 µm deep. Typical: 50–65% power, 600–1,000 mm/s, 30–50 kHz, 0.05 mm hatch, one or two passes.
Deep engraving. Low frequency for high peak energy, slow speed, multiple passes. The mark is clearly recessed, 0.05–0.2 mm deep after several passes, and can be paint-filled. Typical: 70–85% power, 300–500 mm/s, 20–35 kHz, 0.02–0.04 mm hatch, three to five passes.
Two metallurgical cautions apply. First, annealing and melting both heat the steel in air; at the surface, chromium is consumed to form the oxide, leaving a locally chromium-depleted layer. On 304 in a corrosive environment, that is a corrosion initiation site. Deep-engraved and melted marks should be passivated (citric or nitric, per ASTM A967) if the part is going into service outdoors, in food equipment or in a medical device. Second, the recast layer at an engraved wall is harder and more brittle than the base metal and can contain micro-cracks; on a fatigue-critical part, that is a notch, and the next section but one deals with what notches do.
The alloy matters. 304 and 316 mark similarly but not identically; 316's molybdenum shifts the oxide colour. Ferritic 430 marks darker and more readily than austenitic grades. Polished surfaces reflect more and mark lighter; bead-blasted or brushed surfaces absorb more and mark darker. If the drawing says "laser mark per sample", the sample has to be the same alloy and finish as production.
Colour marking with MOPA
The coloured marks on stainless steel tumblers and knives are not a coating and not a pigment. They are a thin oxide film, and the colour comes from interference.
A MOPA source separates the seed pulse from the amplifier, so pulse width and repetition rate can be set independently. That control lets the operator deposit heat in a way that grows an oxide of a specific thickness instead of vaporising the surface. Oxide thickness on 304L has been measured from about 20 nm to roughly 500 nm across the colour range, using a 120 ns fibre laser at 225 kHz. For a film of refractive index n and thickness t, constructive reflection at wavelength \lambda occurs approximately where
The half-order term comes from the phase shift at the metal interface. With n \approx 2.2 and \lambda = 500 nm, the first three constructive thicknesses are 57, 170 and 284 nm. Because the film grows through several orders, the same parameter set can produce gold at one thickness, purple at another and blue at a third — and because the condition depends on \theta, the colour shifts as the part is tilted. That angular dependence is the signature of a genuine interference film, and it is also why a colour match cannot be judged from a photograph taken at one angle.
Parameter logic for colour is different from marking logic:
- Pulse width controls how much heat stays in the surface. Long pulses (tens to hundreds of nanoseconds) grow oxide; short pulses (2–10 ns) ablate and remove it.
- Frequency sets pulse energy for a given average power and the pulse overlap.
- Speed sets the accumulated fluence per unit length — the actual driver of film thickness.
- Hatch must be tight enough for full coverage; 0.001–0.003 mm is typical, which is why colour marking is slow.
- Focus must be controlled to a few tenths of a millimetre, and the surface must be flat across the field.
Starting points on 304 stainless with a 30 W MOPA (JPT M7-class source, 0° fill) look like this:
Colour · Speed · Power · Frequency · Pulse width · Hatch · Passes
Magenta · 1,000 mm/s · 55% · 360 kHz · 45 ns · 0.002 mm · 1
Champagne · 1,500 mm/s · 60% · 360 kHz · 45 ns · 0.002 mm · 1
Bright blue · 2,000 mm/s · 70% · 200 kHz · 4 ns · 0.002 mm · 1
Light green · 1,500 mm/s · 60% · 360 kHz · 45 ns · 0.001 mm · 1
Dark olive · 800 mm/s · 35% · 120 kHz · 150 ns · 0.001 mm · 2
These are starting points, not recipes. Colour is the least transferable process in marking: the same numbers on a different machine, lens, alloy lot or surface finish will land on a different oxide thickness, and therefore a different colour. Production colour work needs a qualification panel per substrate lot, a fixed focus datum, and acceptance under defined lighting at a defined angle. Where colour is decorative, that is manageable. Where it is a brand match across suppliers, it is a specification problem before it is a laser problem.
Aluminium and anodised aluminium
Bare aluminium absorbs 5–10% at 1064 nm, so the standard fibre mark is a light grey-white frosted area from melting and resolidification. It is readable but low contrast. A MOPA source with 2–10 ns pulses at 300–600 kHz can grow a fine, optically dark oxide that reads black on bare aluminium — the highest-contrast mark available without anodising, and one that a Q-switched source cannot reliably reproduce.
Anodised aluminium is a different substrate and a much better one. Type II sulfuric anodise is 5–25 µm thick; Type III hard anodise is 25–50 µm. The coating is porous before sealing and holds dye in the pores. A 1064 nm beam passes through the clear oxide and is absorbed by the dye and the metal beneath, so two mechanisms are available:
- Bleaching or removing the dye leaves clear or white oxide over bright metal — a white mark on black, red or blue anodise. This is the highest-contrast, most repeatable mark in the process.
- Short-pulse MOPA or UV can darken clear anodise by forming a sub-surface oxide without breaching the coating, producing black on silver.
Typical starting points with a 20 W Q-switched source:
Finish · Power · Speed · Frequency · Passes
Black Type II · 40–60% · 1,000–2,000 mm/s · 60–100 kHz · 1–2
Coloured Type II · 40–60% · 1,200–2,500 mm/s · 60–100 kHz · 1
Clear Type II · 50–70% · 800–1,500 mm/s · 40–80 kHz · 1–2
Type III hard · 60–80% · 600–1,200 mm/s · 40–60 kHz · 2–4
The mark depth is a few micrometres up to about 20 µm, the same order as the coating, so a well-controlled mark stays inside the anodise and leaves the corrosion protection intact everywhere except the marked cells. Over-power and you breach the coating to bare aluminium; that is cosmetically acceptable on a nameplate and unacceptable on a marine fitting. Clear anodise is the difficult case: there is no dye to remove, so contrast is weak unless the process is tuned for a dark sub-surface mark.
Plastics: absorption is a formulation problem
Most polymer backbones do not absorb at 1064 nm. The beam passes through, or heats the surface weakly and unpredictably. What makes a plastic markable is what is in it: carbon black, glass fibre, mineral filler, titanium dioxide, certain pigments and flame retardants, or a purpose-designed laser additive at 0.01–3.0% by weight.
Two contrast mechanisms dominate:
- Carbonisation — the polymer chars to a dark mark. Aromatic polymers (ABS, PC, PBT, PET) char readily.
- Foaming — rapid heating traps gas bubbles in a thin surface layer, which scatters light and reads white against a dark part. Common in polyolefins and filled nylons.
Polymer · Fibre 1064 nm · UV 355 nm · CO₂ 10.6 µm · Notes
ABS · Good · Good · Fair · Chars dark; foams light on dark grades
Polycarbonate · Excellent · Excellent · Fair · Watch stress crazing after marking
PA / nylon · Moderate · Good · Poor · Glass-filled grades mark well; natural needs additive
PBT / PET · Good · Good · Fair · Filled grades better
POM (acetal) · Very poor · Fair · Poor · Unzips to volatiles; hard to mark
PP / PE · Poor · Fair · Poor · Additive effectively mandatory
PMMA (acrylic) · Poor · Good · Excellent · Clear acrylic transmits 1064 nm
PVC · Not recommended · Not recommended · Not recommended · Emits HCl; corrosive to optics and machine
The processing window is narrower than for metals because the damage mechanisms are chemical. Over-marking polycarbonate produces stress crazing that appears hours later; over-marking nylon produces a rough, fibre-exposed mark; over-marking a dark part produces a white foam mark where a subtle grey was wanted. Short pulses (2–10 ns) and high frequency keep the heat at the surface; 20–50 ns is a common range for nylon contrast.
Lot-to-lot variation is the hidden cost. A colour change is a new qualification, because the pigment that gives the part its colour also competes with the laser additive for absorption. Two batches of "the same" black polycarbonate can mark with visibly different contrast if the carbon black loading differs. Qualify the actual resin, not the family.
Everything else: glass, wood, coatings, ceramics
CO₂ lasers own the non-metal world because 10.6 µm is absorbed at the surface of materials that are transparent at 1 µm. Soda-lime glass absorbs about 94% at 10.6 µm; the beam induces localised micro-fractures that scatter light and read as a frosted white mark. A fibre laser at 1064 nm passes straight through glass and marks nothing useful — the wavelength is wrong, not the power.
Wood, leather, paper and cardboard char or ablate under CO₂, producing dark marks whose depth and edge quality depend on power, speed and air assist. Ceramics mark by glazing or ablating the surface; glazed tiles need the glaze composition to be known before promising a colour. Powder-coated and painted metals mark by ablating the coating to reveal the substrate or an intermediate layer, which is a completely different contrast mechanism from annealing the metal — and one that leaves an exposed edge for corrosion unless the coating is specified for it.
The code is the product: DPM, UDI and grade B
A logo can be judged by eye. A serial number or a UDI code cannot. Direct-part marking is verified against a standard, and the standard is not "it scans with my phone".
There are two families of grading. ISO/IEC 15415 grades printed symbols; ISO/IEC TR 29158 (AIM DPM) adapts that method to direct marks, where contrast is low, cells are connected or dot-formed, and illumination angle matters. Grades run 0 to 4, where 4 is best and 3 is a B. The overall grade is the lowest of the measured parameters — symbol contrast, modulation, fixed pattern damage, axial nonuniformity, grid nonuniformity, unused error correction and decode. A single bad parameter drags the whole symbol down.
MIL-STD-130 calls for a 2D Data Matrix that verifies to grade B or better; medical device UDI (21 CFR Part 830, EU MDR) requires a permanent mark on reusable devices and the same kind of verification. A supplier who promises "permanent laser marking" without a grade is promising an opinion.
The geometry is where marking and metrology meet. A 10 × 10 mm Data Matrix with 16 modules has a 625 µm module; at a 46 µm spot that is 13 spots across each cell, which is generous. A 2 × 2 mm code with 12 modules has a 167 µm module — 3.6 spots across a cell, which is marginal once the mark spreads, the surface is rough, or the reader aperture is smaller than the module. ISO/IEC TR 29158 recommends an effective aperture of 80% of the minimum X-dimension, and the minimum X-dimension for Type A DPM marks on small medical instruments is 0.100 mm. Below that, the code may decode in the lab and fail in the field.
Practical rules for a code that grades:
- Cell fill: the hatch spacing must be a fraction of the module, not of the field. 0.01–0.02 mm hatch on a 0.5 mm module gives solid cells; 0.05 mm hatch leaves stripes that reduce modulation.
- Contrast: ISO/IEC 15415 grades symbol contrast at ≥70% for A, ≥55% for B, ≥40% for C and ≥20% for D. On metal, an anneal mark rarely reaches the top grades; a white-on-black anodised mark does.
- Quiet zone: keep at least one module of unmarked surface around the symbol. A code etched into a corner with a neighbouring feature in the quiet zone will fail fixed-pattern damage.
- Verification angle: DPM verification is done at a defined illumination angle (45° is the default, and other angles must be reported). A code that grades A under coaxial light and D under 45° is not a grade-A code.
- Reader: use a verifier, not a phone. A phone camera can decode a symbol that a production scanner rejects.
Fatigue, hardness and the marks you must not make
A laser mark is a surface defect, and on a cyclically loaded part a surface defect is a crack nucleus. The data on titanium is the clearest warning in the literature. In a 2023 study of medical-grade titanium marked with a 1064 nm source, oxidative laser marking produced surface melting and a network of cracks extending into the heat-affected zone, with oxygen-stabilised α-phase beneath. The fatigue endurance limit fell from about 750 MPa to 330 MPa for commercially pure titanium — a 56% loss — and from about 1,150 MPa to 250 MPa for Ti6Al4V, a loss of roughly 80%. One higher-energy parameter set reduced the CP-Ti endurance limit to about 100 MPa, an 85% loss. Fracture initiated at the mark in every marked specimen.
This does not mean UDI marking is impossible on implants; it is mandatory. It means the mark has to be placed where the alternating stress is low, made with the lowest energy that achieves the required grade, and validated on the actual geometry. The same logic applies to any high-cycle part: connecting rods, spring leaves, turbine blades, pressure-cycle vessels. Keep marks off fillets, off thread roots, off the tensile side of a bending member, and off cutting edges of tools.
Hardened steel adds a second mechanism. Tempering is time-at-temperature, and a laser mark is a local tempering cycle. A mark on a 60 HRC tool or a case-hardened gear tooth can leave a softened band tens of micrometres deep; it will not fail today, but it will wear first. On carbide inserts, the cobalt binder is the weak link: marking the rake face is a fast way to seed thermal cracks. Mark the shank, not the cutting edge.
Safety and fume
A fibre marker is a Class 4 laser product unless it is enclosed. The 1064 nm beam is invisible, and a specular reflection off a polished stainless surface retains enough power to cause retinal injury before the blink reflex. The controls are not optional:
- Enclosure and interlock — a Class 1 marking cabinet with a door interlock that stops emission is the default for production. Open-format markers need a controlled area, a key switch, a beam stop and a written SOP.
- Eyewear — the required optical density is OD = \log_{10}(H_0/\mathrm{MPE}), where H_0 is the worst-case exposure and MPE is the maximum permissible exposure at that wavelength and pulse duration. For a 100 W Q-switched Nd:YAG at 1064 nm, intrabeam viewing for 600 s calls for OD 5. Eyewear must be rated for the pulse regime, not just the wavelength; EN 207 LB ratings encode both.
- Reflections — mark on a fixture that captures the beam, not on a bare table. A shiny cylindrical part can throw a reflection across the room.
- Fume — this is the hazard that gets ignored. NIOSH sampling of laser marking plumes found hydrochloric acid, benzene, styrene, methyl methacrylate and vinyl chloride from PVC; benzene, toluene, styrene, benzoic acid, phenol and acetophenone from PET, with carbon monoxide at 90–100 ppm; and particle counts at 0.3 and 1.0 µm more than ten times background for polymers. The extraction has to be at the mark, not at the ceiling: a fume arm with a hood within 100 mm of the interaction, ducted outside or through a suitable filter, and never recirculated into the room.
- Materials to refuse — PVC, PTFE and other halogens, and any unknown plastic. HCl and HF attack optics, bearings and lungs. "It marks nicely" is not a risk assessment.
Economics: what a mark costs
A 20 W fibre marker in India starts around ₹1.45 lakh; a 30 W table-top is ₹1.60–1.65 lakh, and industrial 30 W systems run to ₹2.7 lakh. The source itself has a published MTBF around 100,000 hours, with end of life defined as roughly a 20% loss of output power rather than a hard failure. That is a long-lived asset; the cost driver is utilisation, not consumables.
Take a ₹2 lakh machine, five-year life, 2,000 hours a year at 50% utilisation: depreciation is ₹40/h; power at 0.5 kW and ₹8/kWh is ₹4/h; maintenance and optics ₹10/h; operator at ₹150/h. That is about ₹204/h, or ₹0.057/s.
A 10 × 10 mm solid mark at 0.02 mm hatch and 1 m/s takes 5 s of beam time. A Data Matrix with tight hatch and a logo might take 10 s. With 20 s of loading, focusing and unloading, a part is 25–30 s, or about ₹1.4–1.7. Setup — fixture, program, first-off check — is 5 minutes, which adds ₹0.17 per part over a 100-part batch and ₹1.70 over ten.
That is cheap against a printed label (consumable plus application labour) and competitive with pad printing for small marks, with two caveats. First, marking is a serial process: doubling the marked area doubles the time, so large-area coverage is where laser loses to screen printing or labels. Second, the expensive part of marking is often the fixture and the verification, not the beam. A ₹1.4 mark with a ₹40 fixture and a ₹5 verification is really a ₹46 mark.
Laser is the wrong choice when the part cannot be presented flat within the depth of focus, when the mark must be inside a deep cavity the beam cannot reach, when the substrate is a halogenated polymer, or when the volume is so low that programming and qualification exceed the cost of a label.
A production workflow that holds
- Specify the mark and the substrate — alloy, temper, finish, coating thickness, and the standard the mark must meet.
- Run a matrix, not a guess — a 5 × 5 grid of power and speed at fixed frequency, hatch and focus, on the actual production surface.
- Measure, don't eyeball — L* or contrast for visual marks; a verifier for codes. Photograph the grid with the settings written on each square.
- Lock the optics — record lens focal length, focus offset, hatch, pulse width, frequency and pass count in the work instruction.
- Fixture for height — a Z datum, a flat nest and a clamp that does not flex the part. Depth of focus is a tolerance, and the fixture spends it.
- Clean before marking — IPA wipe; fingerprints and cutting oil change absorptance and colour.
- First-off and in-process checks — grade the first part and a sample every hour; anneal colour drifts with lens temperature and focus.
- Post-process — passivate engraved stainless; deburr if the mark is on a sealing face; do not shot-blast a code after verification.
- Package — protect the marked face; a mark that survives salt spray can still be polished off in transit.
FAQ
Can a 20 W fibre laser mark all metals? No. It marks stainless, mild steel, tool steel, titanium and most plated parts well. Bare aluminium gives a low-contrast grey mark unless a MOPA source is used for a black oxide. Copper and brass absorb only 2–20% at 1064 nm and need green/blue wavelengths or a high-peak-power source for a production-grade mark.
Why is my stainless mark brown or yellow instead of black? The mark is an oxide film, and its colour depends on thickness. Too much heat and the film grows past the dark regime into interference colours; too little and it stays pale. Reduce power or increase speed, or change the hatch, and re-run the matrix. A brown mark on 304 is usually an over-annealed mark, not a contaminated lens.
What is the difference between marking, engraving and annealing? Annealing grows an oxide without melting, leaving a flat, tactile-free mark. Engraving removes material and leaves a recess. Marking is the general term for any of these. The same machine does all three; the difference is peak intensity and focus.
How deep is laser engraving? On stainless, 5–50 µm per pass is typical, and 0.05–0.2 mm after several passes. Deep engraving is a milling operation with a very small tool: it is slow, it leaves a recast layer, and it is not the right process for a 1 mm-deep cavity.
Can laser marking survive salt spray and sterilisation? An annealed oxide mark on stainless generally survives both; a shallow melt mark is less durable. Autoclave cycling attacks marks that depend on surface roughness, and salt spray attacks the chromium-depleted zone around a melted mark. Verify with the actual test — ASTM B117 for salt spray, the device's sterilisation cycle — rather than assuming.
Does laser marking weaken the part? It can, severely, if the mark is on a fatigue-critical surface. Titanium endurance limits have been measured 56–85% lower after oxidative marking, with cracks extending into the HAZ. Place marks in low-stress regions, use the minimum energy that meets the marking standard, and validate on the real geometry.
Can you laser mark clear plastics? Not with a 1064 nm fibre laser — clear PC, PMMA and PET transmit it. Use a UV (355 nm) source or a grade formulated with a laser additive. Clear polycarbonate is also prone to stress crazing after marking, so the parameter window is narrow.
What does a Data Matrix grade B mean? It means the symbol verified to 3.0 under ISO/IEC 15415 or ISO/IEC TR 29158, on a 0–4 scale, with every parameter at 3 or better. MIL-STD-130 and many UDI specifications require grade B or better. A phone that decodes the code is not a grade.
Why does the colour change when I tilt the part? Because the colour is thin-film interference, not pigment. The path difference through the oxide depends on the viewing angle, so the reflected wavelength shifts. That is expected; it is also why colour acceptance must be defined at a fixed angle and light source.
Is a 7,000 mm/s marker really that fast? The scanner can move that fast unloaded, but the beam can only draw a continuous line at v \le f_{rep} d_0. At 30 kHz and a 46 µm spot, that is 1.4 m/s. Above it, the line becomes a series of dots. High repetition rate, not high scanner speed, is what buys marking throughput.
The Short Version
Laser marking is a chain of four numbers: the spot the optics form, the energy each pulse carries, the fraction the material absorbs, and the depth of focus the part can hold. Get those right and the settings follow; get them wrong and no recipe transfers.
The material then adds its own constraint. Stainless anneals, melts or ablates depending on intensity, and its colour marks are 20–500 nm oxide films governed by interference. Aluminium needs a MOPA or an anodised coating to show contrast. Polymers need an additive to absorb at all, and some of them — PVC above all — should never see the beam. Codes add metrology: grade B under ISO/IEC 29158, verified with a real verifier, at a module size the spot can fill. Fatigue adds a limit that no marking standard will tell you: a mark is a notch, and on titanium it can cost 80% of the endurance limit.
The shops that mark well are not the ones with the most watts. They are the ones that treat marking as a surface-engineering process with a metrology step at the end — and write down the lens, the focus, the hatch and the pulse before the first part is marked.
Related reading on FabFlow: Laser Cutting, Laser Welding, Anodizing: the 720 Rule, Surface Finishing Technologies, Injection Molding DFM, Metrology and Dimensional Inspection, and GD&T.